Still deciding? Get samples of $ !
Request Sample
|
| Customization: | Available |
|---|---|
| Product Type: | Rod |
| Carbon Content: | Medium Carbon |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
High temperature chip free forming, friction hot melt drilling technology, short for hot melt drilling technology, is a new thin plate drilling method. It uses the basic physical principle of friction heat generation, in the plate or tube metal workpiece drilling with a boss hole, a molding and no drilling cuttings.
Hot melt drill has a variety of calls, including: hot melt drill, hot drill, no chip extrusion hot melt molding drill, stretch drill, extrusion friction drill, tungsten steel hot melt drill, hard alloy hot melt drill, flow drill, flow drill, fluid drill.
Customization support!
Products description
| Grade | YG8 |
| Cut Diameter(mm) | 9.36 |
| Shank Diameter(mm) | 10.00 |
| Total Length(mm) | 36.3 |
| Density(g/cm3) | 16.8 |
| Hardness(HRA) | 89.5 |
| T.R.S(MPa) | 2320 |
|
Grade
|
Density(g/cm3)
|
Hardness (HRA) |
T.R.S (MPa)
|
Grain size (μm)
|
Composition (%) |
Equal to ISO
|
| YU12 | 14.1~14.15 | .≥92.5 | ≥4000 | 0.2~0.5 | 12% CO 88% WC | K40~K50 |
|
YL10.2
|
14.4~14.6
|
≥92.2
|
≥4000
|
0.6~0.8
|
10% CO 90% WC
|
K20~K30
|
|
YG6X
|
14.85~15.0
|
≥92.0
|
≥3860
|
0.8~1.0
|
6% CO 94% WC
|
K05
|
|
YG15
|
14.0~14.1
|
≥85.0
|
≥2800
|
1.2~2.0
|
15%Co 85% WC
|
K30~K40 |
|
YG10
|
14.5~14.6
|
≥85.5
|
≥2600
|
1.2~2.0
|
10%Co 90% WC
|
K20
|
|
YG8
|
14.65~14.85
|
≥89.5
|
≥2320
|
1.2~2.0
|
8% CO 92% WC |
K20
|
|
YG6
|
14.85~15.05
|
≥90.0
|
≥2150
|
1.2~2.0
|
6% CO 94% WC |
K10
|